PAS-C60 Z (vormals / formerly IGOPAS-C6/100 Z)
mechanical characteristics
| Characteristic | Standard | Unit | Value |
|---|---|---|---|
| Yield stress (+23°C, dry) |
ISO 527-1/-2 DIN 53455 ASTM D 638 |
MPa (N/mm²) | 81 |
| Elongation at break (+23°C, dry) |
ISO 527-1/-2 DIN 53455 ASTM D 638 |
% | 35 |
| Tensile E-modulus (+23°C, dry) |
ISO 527-1/-2 DIN 53455 ASTM D 638 |
MPa (N/mm²) | 2900 |
| Max. permissible pressure load (continuous) | Faigle | MPa (N/mm²) | 12 |
| Charpy notched impact strength (+23°C, dry) |
ISO 179 DIN 53453 |
kJ/m² | 3.5 |
| Charpy impact strength (+23°C, dry) |
ISO 179 DIN 53453 |
kJ/m² | No Break |
thermal characteristics
| Characteristic | Standard | Unit | Value |
|---|---|---|---|
| min. Operating temperature (continuous) | °C | -30 | |
| max. service temperature (continuous) | °C | 90 | |
| max. service temperature (short-term) | °C | 170 |
combustibility characteristics
| Characteristic | Standard | Unit | Value |
|---|---|---|---|
| UL94 flammability | IEC 60695-11-10 | class | HB |
electrical characteristics
| Characteristic | Standard | Unit | Value |
|---|---|---|---|
| Surface resistivity (dry) |
DIN IEC 60093 (DIN VDE 0303-30) ASTM D 257 |
Ω | 10^13 |
physical characteristics
| Characteristic | Standard | Unit | Value |
|---|---|---|---|
| Density, Gross density |
ISO 1183 DIN 53479 ASTM D 792 |
g/cm³ | 1.15 |