Material quality - Differential scanning calorimetry (DSC)

Testing processes


Differential scanning calorimetry (DSC)

test device


Perkin Elmer DSC 6

Differential scanning calorimetry (DSC) provides a simple method of precisely identifying materials and their thermal properties, such as the glass transition temperature, melting temperature and even the degree of crystallinity. Furthermore, the implicit wanted and unwanted energy states are also displayed. This thermal analysis shows the behaviour of the material when heat is absorbed or given off.